Florida Outdoor Exposure Testing

Accelerated Lab
Q-Lab Florida’s 120,000 m2 outdoor weathering site and 900 m2 indoor accelerated testing lab.

Q-Lab Florida

Q-Lab Florida has more specimens on test than any other outdoor weathering facility in the world.  Q-Lab Florida is located south of Miami on the southern tip of Florida, in the only true subtropical region in the continental United States. We offer natural outdoor exposure testing, accelerated laboratory testing and specimen evaluation services at Q-Lab Florida.  These contract test services are ISO 17025 accredited.

Why Florida?

Florida is the internationally recognized benchmark location for outdoor exposure testing. Florida subtropical weathering exposures are not only realistic, they are also accelerated. One year of Florida sunshine can equate to several years of weathering elsewhere. Our Florida site has high-intensity sunlight, high annual UV, high year round temperatures, abundant rainfall and very high humidity.

It is this synergistic effect of UV, moisture and heat that makes Miami the ideal location for testing durability of materials in outdoor environments.

The extremely sunny, humid, and warm climate has been proven especially useful for certain types of testing including:

  • Color change, fading, and gloss loss
  • Cracking, peeling, chalking, and blistering
  • Mechanical strength loss and physical deterioration
  • Moisture sensitivity of products like coatings, building materials, and some plastics
  • Biodegradation, including mold, mildew, fungus and algae
  • Accelerated corrosion testing

A Variety of Different Exposure Techniques

Various specimen mounting and exposure techniques are available for natural outdoor exposure testing in Florida:

  • Direct Exposure:
    Direct exposures are used to test many exterior-use materials, such as industrial coatings.  Specimens are securely mounted with their front surface facing the sun. Different exposure angles and mounting methods are used for different applications.
  • Under Glass:
    These exposures are used to test interior-use materials, such as textiles and printing inks.  Specimens are behind 3 mm window glass which will filter out short-wave UV.  Exposures are typically at 45º.
  • Black Box:
    These tests reproduce conditions found on the horizontal surfaces of a vehicle, including higher temperatures and wet times.  Under glass black box exposures are used to test interior automotive materials.
  • AIM Box (Automotive Interior Materials):
    These under glass exposures simulate the environment inside an automobile and are suitable for mounting larger components like dashboards.  Some AIM boxes feature solar tracking.
  • Salt-Accelerated Outdoor Corrosion: 
    Direct exposures with salt spray can produce fast and realistic corrosion, particularly for coated metals.
  • Mildew Tests:
     In this Florida exposure, panels are typically positioned at a 90º north to reduce sunlight, decrease surface temperatures, and increase moisture.  In addition, specimens may be placed near or under vegetation to promote growth.

The specific type of specimen mounting technique and exposure angle both have a significant effect on solar energy dosage, specimen temperature, and time of wetness. For a full description, see LL-9025 - Outdoor Weathering Exposure Procedures, or contact Q-Lab to discuss which option is suitable for your test program.

Florida Weathering & Corrosion Test Methods

Florida outdoor exposure testing meets a variety of weathering and corrosion test methods, a small portion of which are listed below.  Visit our Standards Page or contact Q-Lab for a more complete list.

  • Direct & Under Glass Exposures (ASTM G7, G24, D1435)
  • Black Box (ASTM D4141; GM 9163P)
  • AIM Box (GM 9538P, 7455M, 7454M, 3619M; GMW 3417)
  • Natural Atmospheric Corrosion (ASTM G50)
  • Salt Accelerated Corrosion - SCAB (ASTM D6675)

Natural exposure testing is an essential part of any weathering and light stability test program.  Even if you perform accelerated laboratory weathering testing, you should also perform natural outdoor testing. Furthermore, many companies test their products outdoors in both Florida and Arizona.

  • Q-Lab Florida

    Q-Lab Florida has more specimens on test than any other outdoor weathering facility in the world.

  • Automotive Exposure Testing

    Curved automotive body panels are great candidates for outdoor exposure testing in Florida.

  • Paint & Coatings Exposure Testing

    Q-Lab Florida maintains the capability to mount specimens in almost any orientation including vertical, which is most appropriate for wood siding shown here.

  • Under Glass Exposure Testing

    Sub-frames with window glass protect interior materials tested in "under glass" exposures.

  • Black Box Exposure Testing

    High temperatures are a major factor in Florida exposure tests. Using a "black box" increases the temperature of the specimens even more.

  • AIM Exposure Testing

    These AIM Boxes are used to test materials for automotive interiors. They can hold large, 3D parts like instrument panels.

  • Q-Lab Florida Is The World's Largest Outdoor Weathering Facility

    Q-Lab Florida has the most southerly exposure of any outdoor weathering facility in the United States.

  • Salt Spray Corrosion Testing

    Specimens in salt accelerated corrosion tests are sprayed with a salt solution twice per week.

  • Paint Exposure Testing

    There are many different ways to expose specimens in Florida, depending on specimen size and shape, and which test method is being followed.

Technical Bulletins

Technical Articles

Product Brochures

Specification Bulletins

 

Test Services

Contact Us

Q-Lab Phone Numbers

USA: +1-440-835-8700
Florida & Arizona Test Services: +1-305-245-5600
UK/Europe: +44-1204-861616
Germany: +49-681-857470
China: +86-21-5879-7970

 
View Full Site