RH and Shower Functions
The Q-FOG model CRH can ramp to and maintain a defined RH value and temperature through the use of an air preconditioner, an air control module, and special atomizing humidification nozzles. Deionized (DI) water is required for proper operation.
The Shower Function in the Q-FOG CRH is used for some automotive test specifications. A user-adjustable volume of solution is uniformly sprayed onto specimens through specially positioned spray nozzles. The Shower Function offers the following advantages:
- Nozzles are mounted to either a stationary shower module in the chamber center or a top-mounted swaying shower bar. The stationary shower module can be easily removed when using the Fog Function
- Spray droplets are much bigger, flow rates are much higher, and shower times are much shorter than the atomized solution mist in the Fog Function
- Shower on/off times can be directly programmed to allow for excellent control of corrosion rates
Precise Control of Fog Dispersion
The Q-FOG CRH cyclic corrosion chamber has superior fog dispersion compared to conventional systems, which cannot vary volume and distance independently. A variable speed peristaltic pump controls the amount of corrosive solution delivered to the fog atomizer, while the air pressure regulator controls the distance of the “throw.” Note that purified water is required for proper operation of Q-FOG corrosion testers.
Solution Reservoir
Space utilization is maximized and maintenance is minimized with the Q-FOG tester's internal solution reservoir. The 120 liter reservoir has enough capacity for running most tests for 7 days or more. The reservoir has an integral particulate filter and a built-in alarm to alert the operator when the solution is low. The integrated reservoir can optionally be connected to an external tank.
Rapid Ramp Heater for Fast Temperature and RH Cycling
Q-FOG testers can change temperatures exceptionally fast because of their unique internal chamber heater and their high volume cooling/dry-off blower. An additional air heater allows very low humidity dry-off exposures. Conventional chambers with water jackets cannot cycle rapidly because of the thermal mass of the water, nor can they produce low humidity.
If fast heating or dry-off conditions are required, as prescribed in test standards ISO 11997 and automotive CCT-type tests like JASO M609, the CRH model can be configured with Rapid Ramp Heaters. This Rapid Ramp Heater system enables quick temperature and relative humidity transition in a fully- loaded chamber in order to meet these demanding automotive test standards unconditionally.Calibration
The Q-FOG CRH tester’s chamber temperature and RH sensors should be calibrated by the user every six months to ensure accurate and consistent results.
Calibrating the temperature and RH sensors takes only a few minutes. It requires simple tools, a calibrated reference thermometer, and an insulated container.
Easy Programming and Specimen Mounting
Test conditions, time, and temperature are controlled by a built-in microprocessor. A remarkably simple user interface featuring dual, full-color touch-screens allows for easy programming and operation in 17 languages. The operator can quickly create new cycles, or run any of the pre-programmed cycles. The Q-FOG controller includes complete self-diagnostics, including warning messages, routine service reminders, and safety shutdown.
Q-FOG CRH units come equipped with a viewing window in the side of the lid and an internal light to allow easy monitoring of the test conditions.
Q-FOG testers have a low belt line and an easy-opening lid for easy specimen mounting. For Q-FOG testers with the stationary shower module (“S” models), the 600 model has a capacity of 160 test panels of 75 × 150 mm in size. The 1100 model has a capacity of 240 test panels. For Q-FOG testers with the top-mounted swaying shower bar (“T” models), the 1100 model has a capacity of 230 test panels.
Affordable
Q-FOG cyclic corrosion testers offer state of the art corrosion testing technology, reliability, ease of operation, and easy maintenance – all at a remarkably affordable price.