The QUV accelerated weathering tester can be used to test a variety of specimens. Coatings, plastics, and films are easily accommodated in the QUV tester using standard flat panel specimen holders. Other specimens can be mounted using specialty holders. Q-Lab also offers custom specimen holders for unique needs. All of Q-Lab’s panel holders are designed to meet the requirements of ASTM G154 and other international standards.
The QUV chamber can accommodate a variety of sample types, but three principles should be considered when mounting odd-shaped specimens:
- To insure uniformity of UV exposure, the surface of the test sample should be in the standard sample plane, 50 mm from the lamps.
- The samples and their holders must seal off the side of the QUV tester to prevent vapor from escaping from the chamber.
- The samples are mounted at the wall of the chamber so that room air cooling causes condensation. Samples should have good thermal contact with any backer present. Highly insulating samples thicker than 6mm may require special attention.
See LU-8001 - QUV Sample Mounting
Q-SUN Specimen Holders and Mounting Guidelines
The Q-SUN Xe-2 has a large specimen capacity within a rotating rack design. Textiles, thin films, coatings and other flat samples are very easy to install and remove. It is not recommended to mount large, 3D parts in the Xe-2 tester.
The Q-SUN Xe-1 and Xe-3 tester’s flat specimen mounting system offers the flexibility to test many sizes, shapes and types of specimens. Three-dimensional specimens such as parts, components, bottles and test tubes can be placed directly onto the specimen tray. The near-horizontal specimen tray is also useful for testing materials that flow at elevated temperatures, for materials exposed in petri dishes and for “ponding” in roofing applications.
Holders are available in a number of sizes to accommodate traditional flat specimens, like panels and plaques. Bottle holders, textile holders and special mountings are also available. 3-D specimens can be placed directly on the specimen tray and in most cases do not require a specimen holder.
The Q-SUN Xe-1 and Xe-3 test chambers can accommodate a variety of sample types, but three principles should be considered when mounting odd-shaped specimens:
- To insure uniformity of exposure, the surface of the test sample should be in the standard sample plane, at roughly the same height as the black panel temperature sensor.
- Care should be taken to prevent shadowing of the black panel temperature sensor with large, 3D samples; shadowing can lower the black panel’s temperature, causing the heater in the unit to stay on longer than normal.
- High airflow through the chamber makes it necessary to secure lightweight specimens
See LX-5047 - Q-SUN Specimen Mounting
Q-FOG Specimen Holders & Mounting Guidelines
The Q-FOG cyclic corrosion tester has a large specimen capacity and flexible specimen mounting scheme. Flat specimens are typically mounted in test panel racks, which are slotted at a small backward angle. Maximum weight per rack is not to exceed 113 kg (250 pounds). Larger, three-dimensional parts are typically suspended from a hanging rod, using hooks that are provided. Maximum weight per rod is not to exceed 45 kg (100 pounds).
See LF-8151-SM - Q-FOG Specimen Mounting.
QUV Part Numbers for Specimen Mounting
- V-131.3-K QUV 75mm Panel Holder Kit, set of 25
- V-131.4-K QUV 102mm Panel Holder Kit, set of 18
- V-131.6-K QUV 150mm Panel Holder Kit, set of 13
- V-4960-X QUV Small 3D Part Holder, exposes parts up to 75 x 25 x 324 mm, single holder
- V-4961-X QUV Large 3D Part Holder, exposes parts up to 495 x 25 x 324 mm, single holder
- V-4962-X QUV Adjustable 3D Box for Wood, exposes parts up to 495 x 38 x 324, single holder
Q-SUN Xe-1 Part Numbers for Specimen Mounting
- X-10115-X Q-SUN Flat Specimen Holder, holds 2 specimens on a single holder
- X-10113-K Q-SUN Xe-1 Specimen Holder Kit, set of 8
- X-10183 Q-SUN Narrow Bottle Holder, 17 x 203mm slot on a 51 x 229 mm single holder
- X-10184 Q-SUN Wide Bottle Holder, 19 x 203mm slot on a 51 x 229 mm single holder
- X-10255-X Q-SUN Textile Holder, holds 2 specimens 51 x 102 mm on a single holder
- X-10264-K Q-SUN Textile Masks, paper masks for 51 x 10 2mm holders, set of 100
Q-SUN Xe-2 Part Numbers for Specimen Mounting
- XR-11008-K Q-SUN Solid Back Specimen Holder Kit, set of 15 + 1/2
- XR-11448-K Q-SUN Open Back Specimen Holder Kit, set of 15 + 1/2
- XR-11291-K Q-SUN Specimen Holder Conversion Kit, allows 2 specimens per holder, set of 15
- XR-11273-K Q-SUN Textile Picture Frame Holder Kit, full height, set of 15 + 1/2
- XR-11168-K Q-SUN Full Height Textile Mask Kit, ISO 105 B02 Method 1, 1/3 & 2/3 masks, set of 15 + 1/2
- XR-11316-K Q-SUN Half Height Textile Mask Kit, ISO 105 B02 Method 1, 1/3 & 2/3 masks, set of 31
- XR-11369-K Q-SUN Full Height Textile Mask Kit, ISO 105 B02 Method 2, 1/4, 1/2 & 3/4 masks, set of 15 + 1/2
- XR-11376-K Q-SUN Half Height Textile Mask Kit, ISO 105 B02 Method 2, 1/4, 1/2 & 3/4 masks, set of 31
- XR-11368-K Q-SUN Blue Wool Holder for ISO 105 B04
- XR-11315-K Q-SUN Picture Frame Textile Holder Kit, half height, set of 31
- XR-11229-K Q-SUN AATCC Textile Masks, paper masks for AATCC TM 16-3, set of 100
Q-SUN Xe-3 Part Numbers for Specimen Mounting
- X-10115-X Q-SUN Flat Specimen Holder, holds 2 specimens on a single holder
- X-10114-K Q-SUN Xe-3 Specimen Holder Kit, set of 26
- X-10183 Q-SUN Narrow Bottle Holder, 17 x 203 mm slot on a 51 x 229 mm single holder
- X-10184 Q-SUN Wide Bottle Holder, 19 x 203 mm slot on a 51 x 229 mm single holder
- X-10255-X Q-SUN Textile Holder, holds 2 specimens 51 x 102 mm on a single holder
- X-10264-K Q-SUN Textile Masks, paper masks for 51 x 102 mm holders, set of 100
- X-10260-K Q-SUN Panel Holder Kit, holds 2 flat specimens 76 x 152 mm on a single holder, set of 10
- X-10261-K Q-SUN Panel Holder Kit, holds 2 flat specimens 102 x 152 mm on a single holder, set of 8
- X-10262-K Q-SUN Panel Holder Kit, holds 2 flat specimens 102 x 203 mm on a single holder, set of 6
- X-10476-K Q-SUN 3D Part Holder Kit, 203 x 203mm adjustable height, set of 5
- X-10609-K Q-SUN Textile Specimen Holder Kit, with 1/3 & 2/3 masks, set of 25
Q-FOG Part Numbers for Specimen Mounting - F-9008-K Q-FOG SSP-600 or CCT-600 Test Panel Holder Kit, set of 8
- F-9011-K Q-FOG SSP-1100 or CCT-1100 Test Panel Holder Kit, set of 10
- F-9014-K Q-FOG SSP-600 or CCT-600 20 mm (3/4”) Hanging Rod Kit, set of 6
- F-9017-K Q-FOG SSP-1100 or CCT-1100 20 mm (3/4”) Hanging Rod Kit, set of 8