一个主要的全球合成纤维生产及供应商正准备使用Q-SUN Xe-3氙灯试验箱来优化其配方中紫外稳定剂的使用量,以实现降低成本的目的。
客户设计了一个实验来测试使用不同量的昂贵的抗紫外稳定剂的效果,看减少使用抗紫外稳定剂如何影响曝晒后的机械强度。从他们的测试可得知,他们能大大减少抗紫外稳定剂在其热塑性纤维配方中的用量,在不降低材料性能的前提下,每个月能节省约10,000美金的花费。
仅做一段时间的测试,客户就可以说,Q-SUN Xe-3氙灯试验箱的成本已经收回来了。